材料と環境 Vol. 57 (2008), No. 2
Backnumber
-
Vol. 73 (2024)
-
Vol. 72 (2023)
-
Vol. 71 (2022)
-
Vol. 70 (2021)
-
Vol. 69 (2020)
-
Vol. 68 (2019)
-
Vol. 67 (2018)
-
Vol. 66 (2017)
-
Vol. 65 (2016)
-
Vol. 64 (2015)
-
Vol. 63 (2014)
-
Vol. 62 (2013)
-
Vol. 61 (2012)
-
Vol. 60 (2011)
-
Vol. 59 (2010)
-
Vol. 58 (2009)
-
Vol. 57 (2008)
-
Vol. 56 (2007)
-
Vol. 55 (2006)
-
Vol. 54 (2005)
-
Vol. 53 (2004)
-
Vol. 52 (2003)
-
Vol. 51 (2002)
-
Vol. 50 (2001)
-
Vol. 49 (2000)
-
Vol. 48 (1999)
-
Vol. 47 (1998)
-
Vol. 46 (1997)
-
Vol. 45 (1996)
-
Vol. 44 (1995)
-
Vol. 43 (1994)
-
Vol. 42 (1993)
-
Vol. 41 (1992)
-
Vol. 40 (1991)
キーワードランキング
21 Dec. (Last 30 Days)
材料と環境 Vol. 57 (2008), No. 2
腐食研究への放射光技術の応用
橋本 保, 佐藤 眞直, 山下 正人
pp. 59-65
DOI:
10.3323/jcorr.57.59抄録
The largest third-generation synchrotron radiation beams show advantages of ultra-bright, highly directional, high energy and variable energy when compared with a conventional X-ray equipment. Recently, the application of synchrotron radiation analysis at SPring-8 has been expanded for the research on corrosion phenomenon, such as, structure analysis of the passive film in stainless steel, the rust layer generated on the weathering steel, etc. This report will introduce the SR-X ray analysis methods suitable for corrosion research and applications by XAFS, XRD, GIXS, HX-PES and others.
他の人はこちらも検索
材料と環境 Vol.53(2004), No.1
材料と環境 Vol.64(2015), No.7
材料と環境 Vol.69(2020), No.3
鉄さびの形成過程と構造変化
鈴木 茂
pp. 66-69
DOI:
10.3323/jcorr.57.66抄録
Recent works on formation processes of iron corrosion products are reviewed. Although green rust (GR) is sometimes observed as intermediate corrosion products of iron based alloys, it is easily transformed to ferric oxyhydroxides such as goethite and lepidocrocite through the aerial oxidation. This is because GR contains ferrous ions which are oxidized to ferric ions in aqueous solution. In particular, the characteristic features of the structure and transformation of GR are overviewed in this paper.
放射光を用いたX線回折による耐候性鋼層状剥離さび層の局所構造解析例
原 修一
pp. 70-75
DOI:
10.3323/jcorr.57.70抄録
A local structural analysis of heavy rust layers with large swelling and laminated layers formed on weathering steel bridges using synchrotron radiation X-ray diffraction (SR-XRD) in SPring-8 have been performed. The main constituent in average composition of the whole layer was spinel-type iron oxide [mainly Magnetite (Fe3O4)] and the mass ratio was 30-40 mass%. In contrast the mass ratio of spinel in its local parts, i.e. outer layer, inter-layer and inner layer position was not higher in common but the mass ratio of β-FeOOH was higher. Therefore it indicates that these heavy rust layers have been composed of many layers of spinel poor, rich and poor - cell (SPRaP-cell). Thus SR-XRD is useful for the analysis of the constituent distribution in the rust layer.
軟X線放射光を用いた溶融Zn-Al系めっき上腐食生成物の構造解析
西原 克浩, 松本 雅充, 木本 雅也, 工藤 赳夫, 内田 仁, 春山 雄一, 神田 一浩, 松井 真二
pp. 76-80
DOI:
10.3323/jcorr.57.76抄録
Structure of the native oxide film and the thin corrosion product films, which formed in the early stage on hot-dip Zn-0.2%Al, Zn-5%Al and Zn-55%Al coatings in humid atmosphere under the presence of NaCl particles, were investigated by means of photoemission spectroscopy (PES) using synchrotron radiation (150 eV) and Al-Kα radiation (1487 eV). In 150 eV, the detection depth of Al2p, Zn3d, Cl3p and O2p electron is below approximately 1 nm, and is a third or less of that in 1487 eV.
As a result, the dominant surface components of the native oxide films were aluminum oxide independent of Al content in Zn coatings. It was found that the dominant component in 1nm depth of thin corrosion product films on Zn-Al coatings was different from those in 4 nm. Thin corrosion product films were composed mainly of zinc oxide, zinc chloride, aluminum oxide, zinc chloride, and the ratio of those components was changed by the Al content in Zn coatings and the depth from surface.
マハラノビス距離を用いた淡水中における亜鉛めっき鋼管の腐食事例の判別
高宮 枝里, 中島 博志, 細谷 清, 高橋 歩, 板垣 昌幸
pp. 89-95
DOI:
10.3323/jcorr.57.89抄録
Diagnosis of water quality for polarity reversal in galvanized steel pipes were carried out by using Mahalanobis Distance (MD). Cooling and heating water quality data (109 data of no corrosion trouble and 20 data of corrosion trouble) and coolant water quality data (173 data of no corrosion trouble and 12 data of corrosion trouble) were used for the diagnosis of water quality.
In the diagnosis of cooling and heating water quality, the misjudgment was 1 among 20 troubled data, thus this diagnosis was high accuracy. In diagnosis of coolant water, the misjudgments were 3 among 12 troubled data. Since many kinds of dosing are implemented in coolant water, dosing influenced the water quality remarkably and the accuracy of diagnosis of water quality using MD decreased.
ゴムから放出される硫黄ガス濃度の推定
南谷 林太郎
pp. 96-101
DOI:
10.3323/jcorr.57.96抄録
Silver, a typical electronic material, corrodes in sulfur gas released from rubber. To evaluate the corrosion damage, we established a method for estimating concentration of sulfur gas released from rubber. Firstly, we showed that the silver corrosion behavior in sulfur gas released from rubber is similar to that in sulfur gas released from sulfur flower using a boxy-vessel test. Moreover, the corrosion product on silver was Ag2S only, and the thickness of the corrosion product increased linearly with exposure time. We also found that the silver corrosion rate in the boxy-vessel test depends on both the corrosion reaction and the diffusion of sulfur gas. The former mainly determines the silver corrosion rate. The corrosion rate was therefore calculated by corrosion analysis considering the sulfur gas diffusion and corrosion reaction. Under the condition that the corrosion analysis assumed an inverse problem, the concentration of sulfur gas released from rubber was estimated from the corrosion rate measured by a pre-experiment. By using the corrosion analysis under the boundary condition of concentration of sulfur gas released from rubber, we can estimate the silver corrosion rate in the space of electronic equipment where silver coexists with rubber. We can therefore verify effective countermeasures against corrosion and ensure the corrosion reliability of electronic equipment.
論文アクセスランキング
21 Dec. (Last 30 Days)
-
Wettability of CaS against molten iron at 1873 K
ISIJ International 早期公開
-
凝固過程における溶鋼中からAl2O3上へのMnSの晶出挙動
鉄と鋼 早期公開
-
-
In-situ Observation of Precipitation and Growth of MnS Inclusions during Solidification of a High Sulfur Steel
ISIJ International Vol.64(2024), No.14
-
-
モデル材料を用いた凝固過程における介在物生成挙動のその場観察
鉄と鋼 早期公開
-
Transition behavior of gas containing suspension from solid-like to liquid-like flows
ISIJ International 早期公開
-
-
Slag-steel reactions in the refining of Advanced High-Strength Steel
ISIJ International 早期公開
-
Chemical and Mechanical Factors on Phosphorus Dissolution Behavior from P-concentrated Slag
ISIJ International Vol.64(2024), No.14
この機能はログイン後に利用できます。
下のボタンをクリックしてください。