論文検索サイト

溶接学会論文集 Vol. 36 (2018), No. 3

ISIJ International
belloff
オンライン版ISSN:
冊子版ISSN: 0288-4771
発行機関: JAPAN WELDING SOCIETY

Backnumber

  1. Vol. 42 (2024)

  2. Vol. 41 (2023)

  3. Vol. 40 (2022)

  4. Vol. 39 (2021)

  5. Vol. 38 (2020)

  6. Vol. 37 (2019)

  7. Vol. 36 (2018)

  8. Vol. 35 (2017)

  9. Vol. 34 (2016)

  10. Vol. 33 (2015)

  11. Vol. 32.2 (2014)

  12. Vol. 32 (2014)

  13. Vol. 31 (2013)

  14. Vol. 30 (2012)

  15. Vol. 29 (2011)

  16. Vol. 28 (2010)

  17. Vol. 27 (2009)

  18. Vol. 26 (2008)

  19. Vol. 25 (2007)

  20. Vol. 24 (2006)

  21. Vol. 23 (2005)

  22. Vol. 22 (2004)

  23. Vol. 21 (2003)

  24. Vol. 20 (2002)

  25. Vol. 19 (2001)

  26. Vol. 18 (2000)

  27. Vol. 17 (1999)

  28. Vol. 16 (1998)

  29. Vol. 15 (1997)

  30. Vol. 14 (1996)

  31. Vol. 13 (1995)

  32. Vol. 12 (1994)

  33. Vol. 11 (1993)

  34. Vol. 10 (1992)

  35. Vol. 9 (1991)

  36. Vol. 8 (1990)

  37. Vol. 7 (1989)

  38. Vol. 6 (1988)

  39. Vol. 5 (1987)

  40. Vol. 4 (1986)

  41. Vol. 3 (1985)

  42. Vol. 2 (1984)

  43. Vol. 1 (1983)

溶接学会論文集 Vol. 36 (2018), No. 3

疲労対策用レーザピーニングの低出力化に関する検討

崎野 良比呂, 佐野 雄二

pp. 153-159

抄録

Laser peening can introduce compressive residual stress on the surface of various materials and, therefore, is effective in enhancing the fatigue strength. This study clarifies whether the laser peening with lower pulse energy comparing to the preceding studies generates compressive residual stress, and whether such stress would account for prolonged fatigue life in the welded zone of high-strength steel HT780. As a result, laser peening condition, which can generate large compressive residual stress on the base metal surface, were selected under the pulse energy of 6, 10 and 20mJ, respectively. With the reduction of the pulse energy, it was observed that the depth of the compressive residual stress tended to decrease. Fatigue lives of the toe of the butt welded joints pretreated by laser peening with the selected conditions were prolonged to the same level of fatigue lives with the pulse energy of 200mJ.

ブックマーク

SNSによる共有

論文タイトル

疲労対策用レーザピーニングの低出力化に関する検討

摩擦攪拌により作製したAl/Steel異種金属テーラードブランクの強度特性と後熱処理の影響

小川 大介, 柿内 利文, 橋場 圭吾, 植松 美彦

pp. 160-166

抄録

Aluminum (Al) alloy, A6061-T6, plate and stainless steel, SUS304, plate with different thicknesses were butt welded by a friction stir welding (FSW) process to fabricate tailored blanks. The Al plate was thicker than the steel plate. The FSW tool was offset to the Al side and the probe was inserted only into the Al plate. The shoulder of the tool was also plunged only into the Al plate because of the different thicknesses of the plates. The microstructural observation and X-ray CT revealed that small steel fragments were dispersed in Al-side stir zone (SZ) due to the scratching of steel side surface by the probe. The hardness of SZ in Al side was lower than the base metal due to the dissolution of hardening precipitates during welding, where the lowest hardness located near the thermo-mechanically affected zone (TMAZ) in Al side. The tensile failure occurred at TMAZ because of the bonding strength between Al and steel was higher than TMAZ. However, the tensile strength of the dissimilar weld was approximately 38% lower than that of the aluminum alloy base metal due to the softening at TMAZ. Post heat treatment increased the hardness at TMAZ, whilst the tensile strength was still about 33% lower than the base metal.

ブックマーク

SNSによる共有

論文タイトル

摩擦攪拌により作製したAl/Steel異種金属テーラードブランクの強度特性と後熱処理の影響

Distribution and reduction in P concentration of submerged arc welding slag

Kazuhiro KOJIMA, Masanori SUZUKI, Toshihiro TANAKA

pp. 167-174

抄録

Submerged arc welding (SAW) is widely used in the fields such as ship buildings and steel pipe production. Recently reuse of SAW slag as a raw material of SAW flux has been discussed, as a measure to reduce costs and to conserve natural resources. The present study investigated distribution of P in the slag and its major origin (i.e., welding wire or base metal plate). It also proposed slag remelting as a method of P concentration reduction of the slag. It was recognized that P was mainly distributed in the matrix and metallic steel particles with only larger diameters. It was also identified that the base metal plate was the main source of P in the slag. Remelting of the slag was proved as a promising method for P concentration reduction of the slag.

ブックマーク

SNSによる共有

論文タイトル

Distribution and reduction in P concentration of submerged arc welding slag

埋設パイプライン円周溶接部における水素応力割れ限界硬さの検討

三津谷 維基, 一色 一希, 小口 憲武, 井上 博之

pp. 175-184

抄録

If the coating of the outer surface of a buried pipeline is damaged by some cause and its cathodic protection is excessive, an electrochemical reaction can produce hydrogen. In order to maintain the load transfer function of a pipeline circumferential weld joint in a hydrogen environment as well, the critical hardness at which a constant strength level is ensured during tensile load was clarified by Slow Strain Rate Testing (SSRT). In cases where the hardness was greater than 320HV, the maximum tensile stress was seen to fall sharply in the hydrogen environment, while in cases where hardness was 320HV or lower, the maximum tensile stress fell approximately only 10% regardless of the welding method. The maximum tensile stress fell sharply when the major material of the pipe was material with a relatively hard structure called lath martensite or bainite. The contribution of upper bainite to the fall of the maximum tensile stress was about 1/3.5 of that of lath martensite. From the results of measurement by EBSD, the greater the material's local misorientation, which is a value corresponding to dislocation density, the more conspicuous the fall of the maximum tensile stress under the impact of the hydrogen. It is assumed that the dislocation that exists in steel is an important cause of hydrogen embrittlement, so the empirical tendency-the harder the material, the higher its hydrogen embrittlement susceptibility-has been revealed to be caused by the fact that the harder the material, the greater its internal dislocation. Judging from the above results, if the hardness is 320HV or lower, a constant strength level is maintained under a hydrogen environment regardless of the welding method or the metallic structure.

ブックマーク

SNSによる共有

論文タイトル

埋設パイプライン円周溶接部における水素応力割れ限界硬さの検討

押出Mg-Zn-Y合金の異方性と超音波接合性の関係

星 勇太, 岩本 知広, 東 雄一

pp. 185-192

抄録

Two types of plates, which was cut parallel to the extrusion direction (0°specimen) and perpendicular to the extrusion direction (90°specimen), were prepared for ultrasonic spot welding. After welding, the tensile strength and microstructure of the joints were investigated. For the joints of 0°specimens, the strength was high and the dispersion of its strength was small. In contrast, the joints of 90°specimens were remarkably unstable in strength. To promote the plastic flow at the interface, we put a Mg film as an insert metal between the Mg-Zn-Y plates. After welding of the joints of 90°specimens with the insert metal, we found that the joins were stable in strength. It was revealed that, during the welding, the temperature of the joints with the insert metal was increased compered to the joints without the insert metal.

ブックマーク

SNSによる共有

論文タイトル

押出Mg-Zn-Y合金の異方性と超音波接合性の関係

数値解析によるFSWツール形状が材料流動に及ぼす影響の検討

光藤 健太, 宮坂 史和

pp. 193-198

抄録

The friction stir welding (FSW) is well known as the solid-state joining. Metal materials are not melted during FSW. This paper describes a novel numerical model and calculation method for visualization of material flow during FSW process on A1100 plates. In this numerical model, the particle method as Lagrange approach is mainly employed. In this paper, the numerical model is applied to two FSW processes, and tool's shape change are taken into account. The difference of the material flow around the tool is discussed.

ブックマーク

SNSによる共有

論文タイトル

数値解析によるFSWツール形状が材料流動に及ぼす影響の検討

亜鉛めっき鋼板重ねレーザ溶接時のレーザ加熱による間隙制御とその溶接性への影響

門 格史, 大川 正巳, 篠崎 賢二, 山本 元道

pp. 199-205

抄録

Recently, remote laser welding has come to be used in the automobile manufacture. However, it is well known that welding defects are created depending on the gap amount during laser lap welding of galvannealed/galvanized steel sheets. Pits and blowholes occurr due to vaporization of galvannealed/galvanized coating in the case of a zero or small sheet gap, while burn-through of the upper sheet of the lap joint occurrs in the case of the large gap. In this paper, the sheet gap control process by laser preheating was investigated to avoid defect creations for both cases of the small and large gap during laser welding on the lap joint of galvannealed steel sheets. As a result, it was found that this process could control the gap between steel sheets and improve laser lap weldability of galvannealed steel sheets in both cases of the small and large gap.

ブックマーク

SNSによる共有

論文タイトル

亜鉛めっき鋼板重ねレーザ溶接時のレーザ加熱による間隙制御とその溶接性への影響

母材打撃ハンマーピーニングの高張力鋼への適用

崎野 良比呂, 栗原 康行, 堤 成一郎

pp. 206-211

抄録

Due to the increase of the amount of traffic and the weight of trucks, the fatigue cracks are occurring at the welding joints of steel bridges. This report shows the properties on the surface and depth direction of residual stress of welded joint specimens which were treated by hummer peening in order to study the effect of the hummer peening to the high-strength (HT780) and the conventional (SM490) steel. It was also clarified that the fatigue life of the high-strength steel welded joint specimens which were treated by hummer peening were more than twice as long as the untreated them.

ブックマーク

SNSによる共有

論文タイトル

母材打撃ハンマーピーニングの高張力鋼への適用

この機能はログイン後に利用できます。
下のボタンをクリックしてください。

詳細検索

論文タイトル

著者

抄録

ジャーナル名

出版日を西暦で入力してください(4桁の数字)。

検索したいキーワードを入力して下さい